Chlorine Electrolysis Cell
1.Material: Made of GR1, GR2 titanium material.
2.Coating: Coated with ruthenium and iridium coatings, with a service life more than 5 years. Generation of effective chlorine concentration: ≥9000 ppm.
3.Coating thickness: 0.2-20μm, maintaining stable operation in seawater electrolysis. Chlorine precipitation anode life >5 years, cathode life >20 years.
4.Specification: Available in 50g/h, 100g/h, 200g/h, 300g/h, 1000g/h, 5000g/h and more.
5.Consumption: Salt consumption: ≤2.8 kg/ kg·Cl, DC power consumption: ≤3.5 kwh/kg·Cl.
6.Application: Animal husbandry disinfection, circulating water descaling, disinfection of drinking water, ship ballast water treatment, chemical manufacturing, and swimming pool disinfection.